When using FL2211 for Self-Leveling, dry-blend the powder with cement, sand and other additives before adding water. A typical dosage is 1.5-4.0% by weight of the binder.
Allow a short wet-standing time after mixing so the polymer fully redisperses, then apply with the standard method for Self-Leveling. Avoid excessive dilution, which weakens film formation.
For best results, cure the mortar under controlled humidity for 24-48 h and store FL2211 in a dry place. Contact our team for a formulation sheet tailored to your project.